Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group Kynar Flex® 2900 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group Kynar Flex® 2950 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group Kynar Flex® 3120 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Specific Heat Capacity 0.841 - 1.51 J/g-°C
0.201 - 0.360 BTU/lb-°F
Average value: 1.28 J/g-°C Grade Count:3
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Copyright © lookpolymers.com All Rights Reserved