| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group Kynar Flex® 2950 PVDF Copolymer
(discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer
(discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
|
|||
| Specific Heat Capacity | 0.841 - 1.51 J/g-°C | 0.201 - 0.360 BTU/lb-°F | Average value: 1.28 J/g-°C Grade Count:3 |
|
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||