Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 260 - 290 °C | 500 - 554 °F | |
Plastcom SLOVAMID 66 Y 35 FRY 7 PA66, 35% mineral filling FeaturesPA 66 for injection moulding, chemically reinforced with 35 % mineral filler and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 /3.2 mm/ in accordance wi.. |
|||
Melt Temperature | 250 - 290 °C | 482 - 554 °F | |
Plastcom SLOVAMID® 66 GF 20 HTS PA6 reinforced with glass fiber, heat stabilized, hydrolysis resistant PA66 for injection molding, reinforced with 20% glass fiber, heat stabilized, hydrolysis resistant, for moldings used in the automotive, electrical, building, engineering and hobby industry - holder.. |
|||
Melt Temperature | 250 - 290 °C | 482 - 554 °F | Do not melt above 310°C |
Nilit Nilamon B3 H7 GK 35 15% Glass Fiber, 25% Mineral Reinforced PA6 Description: Nilamon B3 H7 GK 35 provides a combination between low warpage and high stiffness, while retaining a good impact strength. It has a high heat aging resistance, so that it is suitable fo.. |
|||
Melt Temperature | 265 - 290 °C | 509 - 554 °F | |
PolyOne Bergamid™ A70 G30 U Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Melt Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | Recommended |
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | Recommended |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | ISO 294 |
Gromax BFG30-AH00B3 Nylon 6 30% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | ISO 294 |
Gromax BFG30-DN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 250 - 290 °C | 482 - 554 °F | |
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
LATI Latiohm 90/13-09 PD01 G/10 PPOm, 10% Glass Fiber Reinforced Semiconductive/dissipative product based on Modified Polyphenylene Oxide (PPOm). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation prov.. |
|||
Melt Temperature | 275 - 290 °C | 527 - 554 °F | |
Solvay Specialty Polymers Omnix® 9050 Polyamide, High Performance (HPPA), 50% Glass Fiber Omnix® 9050 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties even after moisture ab.. |
|||
Melt Temperature | 260 - 290 °C | 500 - 554 °F | |
Sax Polymers SAXAMID 126F3 Nylon 6, 15% Glass Fiber SAXAMID 126F3 is a polyamide 6 injection-molding-grade reinforced with 15% glass fibers.Information provided by SAX Polymers |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
Tisan TISARBON® 10% Glass Fiber Reinforced Polycarbonate TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind.. |
|||
Melt Temperature | 260 - 290 °C | 500 - 554 °F | |
Tisan TISLAMID® 66 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melt Temperature | 250 - 290 °C | 482 - 554 °F | |
Eastman DuraStar MN621 Polymer, Natural Durastar Polymer MN621 was developed for the medical device industry and contains a mold release It processes easily and requires minimal drying time. It has superior toughness, high clarity and goo.. |
|||
Melt Temperature | 260 - 290 °C | 500 - 554 °F | |
CP-Polymer-Technik Wellamid® 6600 HWUVCP Nylon 66, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | DAM; Injection Molding |
DuPont Performance Polymers Zytel® FE310001 NC010 Nylon 612 Zytel® FE310001 NC010 is a high viscosity polyamide 612 resin that is suitable for extrusion applications, such as monofilaments and tubing.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | DAM |
DuPont Performance Polymers Zytel® RS LC3030 NC010 Nylon 610
(Unverified Data**) Zytel® RS LC3030 NC010 is a renewable sourced polyamide 610 containing a minimum of 60% renewably sourced ingredient by weight. It is an unreinforced, low viscosity grade, developed for extrusion a.. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide AS10 PA66, 50% Glass Bead Reinforced, Injection Molding Staramide AS10 is a 50% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide RF006S-GY9A121 PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006S-GY9A121 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
E-Polymers TEKAMID® TA210MS MoS2 Filled PA66 Resin Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,.. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide RF006K PA66, Glass Fiber Filled, Injection Molded Staramide RF006K is a Radiation Crosslinkable, Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide RF006XXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006XXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006)Information provided by Eurostar. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Melt Temperature | 250 - 290 °C | 482 - 554 °F | |
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Conditioned) Description: Ultramid 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines fl.. |
|||
Melt Temperature | 250 - 290 °C | 482 - 554 °F | |
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Dry) Description: Ultramid 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines fl.. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | Injection Molding/Extrusion |
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Dry) Information provided by BASF |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | Injection Molding/Extrusion |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |