| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
|
Polykemi AB POLYfill PP CPQ10015 FF Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
|
Polykemi AB POLYfill PP CQX10030 R3 Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB
|
|||
| Melt Temperature | 230 °C | 446 °F | |
|
Chevron Phillips 5497 LDPE High Clarity, Bakery Packaging Film Resin
(discontinued **)
Resin Type: HomopolymerCharacteristics: Excellent Openability, Suited for High Speed Converting, Good Clarity. Slip 1000 ppm. Antiblock 10000 ppm.Applications:Bakery Film, Bread BagsProcessing Con..
|
|||
| Melt Temperature | 230 - 260 °C | 446 - 500 °F | Start Point: 250°C |
|
Kingfa JH830 Flame Retardant PC
Features:UL V-0 @ 1.6mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInformation Prov..
|
|||
| Melt Temperature | 230 - 260 °C | 446 - 500 °F | ISO 294 |
|
Gromax BTE25-DN00N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Melt Temperature | 230 - 280 °C | 446 - 536 °F | |
|
Lanxess Durethan® BC 700 HTS DUSXBL 900116 Nylon 6, Impact Modified
PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
|
LATI Latilub 62-15ST PA6
Self-lubricating product based on Polyamide 6 (PA6). Silicone / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Term..
|
|||
| Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
|
LATI Latiohm 62-09 PD01 G/20-V2HF PA6, 20% Glass Fiber Reinforced, Flame Retardant
Semiconductive/dissipative product based on Polyamide 6 (PA6). Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Very good mechanical properties.Availabili..
|
|||
| Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
|
LATI Latistat 62-08 PA6
Dissipative product based on Polyamide 6 (PA6). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S..
|
|||
| Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
|
LATI Latistat 63-08 PA6, Impact Modified
Dissipative product based on Polyamide 6 (PA6), impact modified. Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
|
|||
| Melt Temperature | 230 - 270 °C | 446 - 518 °F | Injection Molding |
|
Styrolution Terluran® HH-112 Q42 Gray 10072 ABS
Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Melt Temperature | 230 - 260 °C | 446 - 500 °F | Injection Molding |
|
Styrolution Terlux® 2802 TR Q434 Transparent MABS
Description: Terlux® 2802 TR Q434 is a new grade with enhanced toughness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
|
Borealis BC650MO Polypropylene Copolymer
BC650MO is a very high impact polypropylene heterophasic copolymer intended for injection molding. This product offers a good UV resistance, further enhanced by pigmentation. This grade features hig..
|
|||
| Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
|
Borealis HD120MO Polypropylene
HD120MO is a polypropylene homopolymer with a good combination of mechanical properties intended for injection molding. Applications: sanitary equipment, caps and closures, and general packagingInf..
|
|||
| Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
|
Borealis Xmod™ GB305HP High Performance 35% Glass Fiber Reinforced
Xmod GB305HP is reinforced with 35% chemically coupled glass fibers and based on a specific Polymer matrix material that is bringing excellent mechanical properties (biaxial impact behavior) as well..
|
|||
| Melt Temperature | 230 - 280 °C | 446 - 536 °F | |
|
Eastman DuraStar DS1910HF Polymer, Natural
Durastar DS1910HF polymer is a high flow grade of Durastar that contains a mold release. Durastar DS1910HF flow lengths are increased 20-40% relative to Durastar DS1010 as shown by spiral flow testi..
|
|||
| Melt Temperature | 230 °C | 446 °F | Optimum; Blow Molding |
|
DuPont Performance Polymers Hytrel® HTR5612BK TPC-ET
(Unverified Data**)
Hytrel® HTR5612BK HTR5612BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal durometer hardness of 54D, is pigmented black with fine particle size..
|
|||
| Melt Temperature | 230 °C | 446 °F | Optimum; Injection Molding |
|
DuPont Performance Polymers Hytrel® HTR8136BK TPC-ET
(Unverified Data**)
Hytrel® HTR8136BK is designed for blow molding or processing by techniques requiring high melt viscosity. It has nominal durometer hardness of 49D, is pigmented black with fine particle size carbon..
|
|||
| Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
|
Azoty Tarnow™ Tarnamid® T-27 CF20 Polyamide 6 20% Carbon Fiber- Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
|
|||
| Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
|
Azoty Tarnow™ Tarnamid® T-27 CF30 Polyamide 6 30% Carbon Fiber - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
|
|||
| Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
|
Azoty Tarnow™ Tarnamid® T-27 GF10 MX10 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T..
|
|||
| Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
|
Azoty Tarnow™ Tarnamid® T-27 Polyamide 6 - Natural
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechanical strength, rigidi..
|
|||
| Melt Temperature | 230 - 260 °C | 446 - 500 °F | Injection-molding/Extrusion |
|
BASF Ultramid® Seal-Fit PA6/66 (Dry)
Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF
|
|||
| Melt Temperature | 230 - 280 °C | 446 - 536 °F | Average value: 257 °C Grade Count:26 |
|
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..
|
|||