Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.0 - 20.0 kV/mm @Thickness 1.00 mm |
381 - 508 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Raschig Group 3535 Epoxy Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IEC 60243-1 |
Raschig Group 5553 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IEC 60243-1 |
Raschig Group 5562 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IEC 60243-1 |
Raschig Group 5563 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IEC 60243-1 |
Raschig Group 6501 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IEC 60243-1 |
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IEC 60243-1 |
Raschig Group 6552 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IEC 60243-1 |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IEC 60243-1 |
Raschig Group MELOPLAS® 150 MF Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IEC 60243-1 |
Raschig Group MELOPLAS® 152 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IC 60243-1 |
Raschig Group MELOPLAS® 152.7 MF Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IEC 60243-1 |
Raschig Group MELOPLAS® 181 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IEC 60243-1 |
Raschig Group MELOPLAS® 181.5 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IEC 60243-1 |
Raschig Group MELOPLAS® 181.5 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IEC 60243-1 |
Raschig Group MELOPLAS® 3025 MF Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu.. |
|||
Dielectric Strength | 17.7 - 20.0 kV/mm | 450 - 508 kV/in | Average value: 18.3 kV/mm Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IEC 60243-1 |
Raschig Group 3572 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis.. |
|||
Dielectric Strength | 18.7 - 20.0 kV/mm | 475 - 508 kV/in | Average value: 19.6 kV/mm Grade Count:3 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
Dielectric Strength | 16.0 - 20.0 kV/mm | 406 - 508 kV/in | Average value: 17.4 kV/mm Grade Count:7 |
Overview of materials for Epoxy, Molded, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Mineral Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Dielectric Strength | 3.10 - 20.0 kV/mm | 78.7 - 508 kV/in | Average value: 11.0 kV/mm Grade Count:9 |
Overview of materials for Phenolic, Novolac, Fabric Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values .. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | DIN 53481 |
Zell-Metall Engineering Plastics Zellamid 1100 at 50% RH Zellamid® 1100 is the registered trademark for Zell-Metalls cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers .. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | DIN 53481 |
Zell-Metall Engineering Plastics Zellamid 1100 MO at 50% RH Improved sliding and self-lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | DIN 53481 |
Zell-Metall Engineering Plastics Zellamid 1100 OIL at 50% RH Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | DIN 53481 |
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |
|||
Dielectric Strength | 12.0 - 20.0 kV/mm | 305 - 508 kV/in | ASTM D149 |
Adamas Adalon® 463 PTFE, 15% Special Polyimide Information provided by Adamas, HPM |
|||
Dielectric Strength | 17.6 - 20.0 kV/mm | 447 - 508 kV/in | DC Breakdown Strength |
China-Yixing Longly Refractories 95 Alumina Ceramic Seals LONGLY's alumina ceramic seals (alumina accounts for 95-99%) can be finished by mirror-polishing process. Because of high mechanical strength, strong chemical corrosion resistance, good air tightne.. |
|||
Dielectric Strength | 0.122 - 20.0 kV/mm | 3.10 - 508 kV/in | Average value: 16.3 kV/mm Grade Count:8 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm @Thickness 1.00 mm |
381 - 508 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Raschig Group 5557 DAP
(discontinued **) Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot h.. |
|||
Dielectric Strength | 1.38 - 20.0 kV/mm | 35.0 - 508 kV/in | Average value: 10.2 kV/mm Grade Count:13 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |
|||
Dielectric Strength | 17.6 - 20.0 kV/mm | 447 - 508 kV/in | DC Breakdown Strength |
China-Yixing Longly Refractories 95 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |