Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Raschig Group MELOPLAS® 152.7 MF

Category Polymer , Thermoset , Melamine , Melamine-Phenolic Copolymer , Phenolic
Manufacturer Raschig Group
Trade Name MELOPLAS®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Raschig Group MELOPLAS® 152.7 MF.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically harmless even after long-term contact with foodstuff. Self-extinguishing (V-0/1,6 according to UL 94). Free of halogens and toxic heavy metals. Supervised according ISO 14528-3 DIN 7708: MF 152.7 ISO 800: MF B11/B12 ISO 14528-3: MF (LD20+MD25) - (LD30+MD15), X, N. Forms: Low dust granulate packed in moisture resistant bags. Standard bag size: 25 kg palletized in 1.000 kg loads or big-bags. Processing: Injection or Compression. Applications: Table ware, Pot-ladles, Noodle sieves. Information provided by the Raschig Group
Physical Properties Metric English Comments
Specific Gravity 1.50 - 1.70 g/cc
1.50 - 1.70 g/cc
ISO 1183
Apparent Bulk Density 0.550 - 0.750 g/cc
0.0199 - 0.0271 lb/in³
ISO 60
Water Absorption <= 2.0 %

@Temperature 23.0 °C,
Time 86400 sec
<= 2.0 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0050 - 0.010 cm/cm
0.0050 - 0.010 in/in
Compression; ISO 2577
0.0080 - 0.013 cm/cm
0.0080 - 0.013 in/in
Injection; ISO 2257
Mechanical Properties Metric English Comments
Ball Indentation Hardness 250 - 300 MPa
36300 - 43500 psi
23°C; ISO 2039
Tensile Strength, Yield 40.0 - 65.0 MPa
5800 - 9430 psi
Compression; ISO 527
50.0 - 90.0 MPa
7250 - 13100 psi
Injection; ISO 527
Modulus of Elasticity 5.00 - 8.00 GPa
725 - 1160 ksi
Injection and Compression; ISO 527
Flexural Strength 90.0 - 120 MPa
13100 - 17400 psi
Compression; ISO 178
100 - 130 MPa
14500 - 18900 psi
Injection; ISO 178
Flexural Modulus 8.00 - 9.00 GPa
1160 - 1310 ksi
Injection and Compression; ISO 178
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Charpy Impact Unnotched 0.600 - 0.900 J/cm²

@Temperature 23.0 °C
2.86 - 4.28 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eU
0.800 - 1.40 J/cm²

@Temperature 23.0 °C
3.81 - 6.66 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Charpy Impact, Notched 0.140 - 0.200 J/cm²

@Temperature 23.0 °C
0.666 - 0.952 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eA
0.150 - 0.200 J/cm²

@Temperature 23.0 °C
0.714 - 0.952 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Thermal Properties Metric English Comments
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
longitudinal; ISO 11359-2
Thermal Conductivity 0.400 - 0.500 W/m-K
2.78 - 3.47 BTU-in/hr-ft²-°F
DIN 52 612
Maximum Service Temperature, Air 135 °C
275 °F
20,000 h; IEC 216/T1
160 °C
320 °F
< 50 h; IEC 216/T1
Deflection Temperature at 1.8 MPa (264 psi) 155 - 180 °C
311 - 356 °F
Injection and Compression; ISO 75-A
Deflection Temperature at 8.0 MPa 110 - 130 °C
230 - 266 °F
Injection and Compression; ISO 75-C
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Shrinkage 1.0 - 1.5 %

@Temperature 110 °C,
Time 605000 sec
1.0 - 1.5 %

@Temperature 230 °F,
Time 168 hour
ISO 2577
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 - 1.00e+12 ohm-cm
1.00e+11 - 1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 - 1.00e+11 ohm
1.00e+10 - 1.00e+11 ohm
IEC 60093
Dielectric Constant 7.0 - 9.0

@Frequency 1.00e+6 Hz
7.0 - 9.0

@Frequency 1.00e+6 Hz
IEC 60250
11 - 16

@Frequency 100 Hz
11 - 16

@Frequency 100 Hz
IEC 60250
Dielectric Strength 15.0 - 20.0 kV/mm
381 - 508 kV/in
IC 60243-1
Dissipation Factor 0.030 - 0.050

@Frequency 1.00e+6 Hz
0.030 - 0.050

@Frequency 1.00e+6 Hz
IEC 60250
0.30 - 0.50

@Frequency 100 Hz
0.30 - 0.50

@Frequency 100 Hz
IEC 60250
Comparative Tracking Index >= 600 V
>= 600 V
CTI; IEC 60112
Processing Properties Metric English Comments
Shelf Life 6.00 Month

@Temperature 15.0 - 25.0 °C
6.00 Month

@Temperature 59.0 - 77.0 °F
Descriptive Properties Value Comments
Arc Resistance 5 Stufe
ASTM D495
Glow wire ignitability test 900/1
IEC 60695 2-13
Glow-wire flammability test 960/1
IEC 60695 2-12
Water Absorption <115 mg
ISO 62; 24h / 23°C