Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 381 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Dielectric Strength 15.0 kV/mm
381 kV/in
ASTM D149
Premix Premi-Glas® 1200H-25 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200H-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go..
Dielectric Strength 15.0 kV/mm
381 kV/in
ASTM D149
Premix Premi-Glas® 2203-22 CR-SX-HT Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2203-22 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL..
Dielectric Strength 15.0 kV/mm
381 kV/in
ASTM D149
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass..
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Lexan® 244R PC
10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release.
Dielectric Strength 15.0 - 20.0 kV/mm
381 - 508 kV/in
IEC 60243-1
Raschig Group 5562 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Dielectric Strength 15.0 kV/mm
381 kV/in
IEC 60112
RedEye On Demand Polycarbonate High Impact Strength & Temperature Resistant for Rapid Prototyping
Polycarbonate (PC) is an actual industrial-grade thermoplastic that is impact-resistant and structurally strong. PC parts are built with a layered manufacturing process utilizing Fused Deposition Mo..
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Lexan® LUX2614G PC (Europe-Africa-Middle East)
Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop..
Dielectric Strength 15.0 kV/mm

@Thickness 2.00 mm
381 kV/in

@Thickness 0.0787 in
IEC 243-1
LATI LAPEX A Polyethersulfone (PES) (UL94 V-0)  (Unverified Data**)
Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist..
Dielectric Strength 15.0 - 20.0 kV/mm
381 - 508 kV/in
IEC 60243-1
Raschig Group 3572 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis..
Dielectric Strength 15.0 kV/mm
381 kV/in
Arkema Group Oroglas® DRT Acrylic, Impact Grade  (discontinued **)
For extrusion and injection molding applications. OROGLAS DRT combines good thermal resistance with an excellent impact resistance.Key features : impact resistance: up to 10 times more impact-resis..
Dielectric Strength 15.0 kV/mm
381 kV/in
Arkema Group Oroglas® HFI-10 Acrylic, Impact Grade  (discontinued **)
OROGLAS HFI-10 is an impact grade that in addition to its superior impact resistance provides an improvement in flow which contribute to improve molding behavior and reduce cycle time.Key features :..
Dielectric Strength 15.0 kV/mm
381 kV/in
4kV/s; ASTM D149
LG Chemical HI835HS PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
Dielectric Strength 15.0 kV/mm
381 kV/in
4kV/s; ASTM D149
LG Chemical HI855HS PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
Dielectric Strength 15.0 kV/mm
381 kV/in
4kV/s; ASTM D149
LG Chemical HI855M PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
Dielectric Strength 15.0 kV/mm
381 kV/in
Wet, step-by-step. ASTM D149
Sumitomo Bakelite North America 3-2-530 Short-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A..
Dielectric Strength 15.0 kV/mm
381 kV/in
Wet, step-by-step. ASTM D149
Sumitomo Bakelite North America 2-530 Short-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Am..
Dielectric Strength 15.0 kV/mm
381 kV/in
ASTM D149
Tipco Tipcolite® VASW 200 Phenolic Compound, Long Glass Fiber, in fluffy form, Medium -Soft Flow & Very High Strength
Dielectric Strength 15.0 - 20.0 kV/mm
381 - 508 kV/in
DIN 53481
Zell-Metall Engineering Plastics Zellamid 1100 OIL at 50% RH
Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces ..
Dielectric Strength 15.0 kV/mm
381 kV/in
Short Time; ASTM D149
Plenco 4311 Phenolic, Granular, Compression Molded
PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized..
Dielectric Strength 15.0 - 50.0 kV/mm
381 - 1270 kV/in
Goodfellow Ruby, Al2O3
Ruby exhibits identical properties to those of sapphire. Small amounts of impurities, especially chromium oxide, give ruby a red coloration. Useful optical range from 150 - 5500 nm.Information pro..
Dielectric Strength 15.0 kV/mm
381 kV/in
IEC 60243-1
DSM Stanyl® TW363 (COND) Nylon 46 Heat Stabilized, Impact Modified (North America)
Information provided by DSM Engineering Plastics.
Dielectric Strength 15.0 kV/mm

@Thickness 2.00 mm
381 kV/in

@Thickness 0.0787 in
ASTM D149
Beijing Chemical Industry KAIFA® S-206 PPS Resin
Glass fiber reinforced and mineral filledInformation provided by Beijing Chemical Industry Research Institute (Group)
Dielectric Strength 15.0 kV/mm
381 kV/in
ASTM D149
Gharda Chemicals Gafone™ B2315GF Polysupersulfone (PSS)  (discontinued **)
Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical..
Dielectric Strength 15.0 - 20.0 kV/mm

@Thickness 1.00 mm
381 - 508 kV/in

@Thickness 0.0394 in
IEC 60243-1
Raschig Group 5557 DAP  (discontinued **)
Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot h..
Dielectric Strength 15.0 kV/mm
381 kV/in
Wet, short term. ASTM D149
Sumitomo Bakelite North America FS-6 CAF Mineral Filled Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type MI..
Dielectric Strength 15.0 kV/mm
381 kV/in
Wet, step-by-step. ASTM D149
Sumitomo Bakelite North America RX® 1-510N Mineral Filled Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ..
Dielectric Strength 15.0 kV/mm

@Thickness 1.60 mm
381 kV/in

@Thickness 0.0630 in
ASTM D149
E-Polymers SEPAZ® K130HF 30% Glass Fiber Reinforced High Flow PPS Resin
Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit..