3M XR8115 Double Coated Paper Tapes

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M XR8115 Double Coated Paper Tapes.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product construction to support demanding application requirements. This product line provides a range of adhesive transfer and double-coated tapes designed for attachment of paper, corrugated, films, foils, fabric plastics and metal. Double Coated (DC) tapes provide a backing for improved handling. Adhesive Transfer Tapes (ATT) provide the thinnest bold lines. The 3M™ X-Series Tape System is manufactured in the United States by 3M.Information provided by 3M
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
Release Liner
152 microns
6.00 mil
Tape
Mechanical Properties Metric English Comments
Peel Strength 0.701 kN/m
4.00 pli
Backside, to Stainless Steel, 180° Peel, 2 mil Al
0.745 kN/m
4.25 pli
Faceside, to Stainless Steel, 180° Peel, 2 mil Al
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Long Term
66.0 °C
151 °F
Short Term
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Carrier Natural Rubber
Adhesive Type Natural Rubber
Liner White Densified Kraft Liner with Red Print