A. Schulman ComAlloy Hiloy® 284 PPO Alloy, Glass/Graphite Reinforced

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Glass/Graphite Reinforced
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Hiloy® 284 PPO Alloy, Glass/Graphite Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.50% Glass/Graphite Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
ASTM D785
Tensile Strength, Ultimate 79.0 MPa
11500 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 126 MPa
18300 psi
ASTM D790
Flexural Modulus 8.20 GPa
1190 ksi
ASTM D790
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.71 J/cm
3.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 146 °C
295 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 141 °C
286 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 260 - 279 °C
500 - 534 °F