| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced |
| Manufacturer | Aclo Compounders |
| Trade Name | Accucomp |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Aclo Accucomp Nylon 66 NY0750L.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.018 cm/cm | 0.018 in/in | MD; ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 121 | 121 | ASTM D785 |
| Tensile Strength at Break | 50.0 MPa | 7250 psi | ASTM D638 |
| Tensile Strength, Yield | 81.98 MPa | 11890 psi | ASTM D638 |
| Elongation at Break | 100 % | 100 % | ASTM D638 |
| Elongation at Yield | 5 % | 5 % | ASTM D638 |
| Tensile Modulus | 3.00 GPa | 435 ksi | ASTM D638 |
| Flexural Strength | 113.0 MPa | 16390 psi | ASTM D790 |
| Flexural Modulus | 3.00 GPa | 435 ksi | ASTM D790 |
| Izod Impact, Notched | 0.374 J/cm | 0.700 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 265 °C | 509 °F | ASTM D789 |
| Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 359 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F |