| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer |
| Manufacturer | Aclo Compounders |
| Trade Name | Accucomp |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Aclo Accucomp Polypropylene CPO406L Copolymer.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | MD; ASTM D955 |
| Melt Flow | 12 g/10 min | 12 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 66 | 66 | ASTM D785 |
| Tensile Strength at Break | 17.0 MPa | 2470 psi | ASTM D638 |
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
| Elongation at Break | 400 % | 400 % | ASTM D638 |
| Elongation at Yield | 6.0 % | 6.0 % | ASTM D638 |
| Tensile Modulus | 1.00 GPa | 145 ksi | ASTM D638 |
| Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
| Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
| Izod Impact, Notched | 1.82 J/cm | 3.40 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C | 169 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 47.8 °C | 118 °F |