| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled |
| Manufacturer | Aclo Compounders |
| Trade Name | Accutech |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Aclo Accutech ABS ABS832G40L Glass Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.35 g/cc | 0.0488 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | MD; ASTM D955 |
| Melt Flow | 0.30 g/10 min | 0.30 g/10 min | ASTM D1238 |
| Ash | 40 % | 40 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 103 | 103 | ASTM D785 |
| Tensile Strength at Break | 95.01 MPa | 13780 psi | ASTM D638 |
| Tensile Strength, Yield | 95.01 MPa | 13780 psi | ASTM D638 |
| Elongation at Break | 4.0 % | 4.0 % | ASTM D638 |
| Elongation at Yield | 3.0 % | 3.0 % | ASTM D638 |
| Tensile Modulus | 5.699 GPa | 826.6 ksi | ASTM D638 |
| Flexural Strength | 145.0 MPa | 21030 psi | ASTM D790 |
| Flexural Modulus | 10.798 GPa | 1566.1 ksi | ASTM D790 |
| Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F |