| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Impact Grade |
| Manufacturer | Adell Plastics, Inc. |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Adell HI-10 Impact Modified PBT.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
| Water Absorption | 0.060 % | 0.060 % | 24 hr immersion; ASTM D570 |
| Linear Mold Shrinkage | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 78 | 78 | ASTM D785 |
| Hardness, Rockwell R | 116 | 116 | ASTM D785 |
| Tensile Strength, Ultimate | 45.0 MPa | 6530 psi | ASTM D638 |
| Flexural Strength | 80.0 MPa | 11600 psi | ASTM D790 |
| Flexural Modulus | 2.10 GPa | 305 ksi | ASTM D790 |
| Compressive Yield Strength | 82.7 MPa | 12000 psi | ASTM D695 |
| Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm |
2.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 210 - 227 °C | 410 - 440 °F | ASTM D789 |
| Deflection Temperature at 0.46 MPa (66 psi) | 138 °C | 280 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |