Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Pebax® MV 1074 SN 01 Polyether Block Amide (PEBA) (Conditioned)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Arkema Group Pebax® MV 1074 SN 01 Polyether Block Amide (PEBA) (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....) Permanent antistatic additive in polymersISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Melt Flow 14 g/10 min

@Load 1.00 kg,
Temperature 235 °C
14 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
Tensile Strength, Yield 9.30 MPa

@Strain 50.0 %
1350 psi

@Strain 50.0 %
50 mm/min
Tensile Modulus 0.0890 GPa
12.9 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 158 °C
316 °F
(Dry)
Vicat Softening Point 121 °C
250 °F
50°C/hr; 50N
Oxygen Index 19.4 %
19.4 %
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.
Electrical Properties Metric English Comments
Surface Resistance 3.00e+8 ohm