| Category | Polymer , Thermoset , Silicone , Silicone Rubber |
| Manufacturer | Arlon |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Arlon 31970XA015 Silicone Rubber Laminate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | Silicone Property; Arlon SQA-TMS-024 |
| Thickness | 178 microns | 7.00 mil | carrier; Arlon SQA-TMS-003 |
| 381 microns | 15.0 mil | overall; Arlon SQA-TMS-003 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 62 | 62 | Silicone Property; ASTM D2240 |
| Tensile Strength, Ultimate | 8.89 MPa | 1290 psi | Silicone Property; ASTM D412 |
| Elongation at Break | 150 % | 150 % | Silicone Property; ASTM D412 |
| Tear Strength | 14.5 kN/m | 83.0 pli | Silicone Property; ASTM D624 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
| Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
| Flammability, UL94 | V-1 | V-1 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 38.5 kV/mm | 977 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 15.0 min @Pressure 0.345 MPa, Temperature 121 °C |
0.250 hour @Pressure 50.0 psi, Temperature 250 °F |
|
| Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Gray |