Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Kasei Tenac® 4012 Homopolymer Acetal Resin

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced
Manufacturer Asahi Kasei
Trade Name Tenac®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Tenac® 4012 Homopolymer Acetal Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Medium viscosity grade, with reduced stiffness and increased elongation through addition of special polymersInformation provided by Asahi Kasei Corporation.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
Asahi Kasei Method
Melt Flow 10 g/10 min
10 g/10 min
ISO 1133 D
Mechanical Properties Metric English Comments
Tensile Strength at Break 66.0 MPa
9570 psi
ISO 527 - 1 & - 2
Elongation at Break 35 %
35 %
ISO 527 - 1 & - 2
Tensile Modulus 2.90 GPa
421 ksi
ISO 527 - 1 & - 2
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179 / 1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 151 °C
304 °F
ISO 75 -1 & -2 flat
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75 -1 & -2 flat
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: