Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® ABS 243

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® ABS 243.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Medium impact, high flow, rigid. Suitable for injection molding of appliances, automotive components, office machines, switch boxes and panels.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Typical value for ABS
Melt Flow 3.5 g/10 min
3.5 g/10 min
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 53.0 MPa
7690 psi
ASTM D638
Flexural Strength 69.0 MPa
10000 psi
ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
ASTM D790
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C
196 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
ASTM D648
Flammability, UL94 V-2
V-2