| Category | Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced |
| Manufacturer | Azoty Tarnow™ (Zaklady Azotowe) |
| Trade Name | TARNOFORM |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Azoty Tarnow™ TARNOFORM 300 SI POM.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.41 g/cc | 0.0509 lb/in³ | ISO 1183 |
| Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 115 | 115 | ISO 2039 |
| Ball Indentation Hardness | 120 MPa | 17400 psi | 358 N; ISO 2039-1 |
| Tensile Strength, Yield | 55.0 MPa | 7980 psi | ISO 527 |
| Elongation at Break | 75 % | 75 % | ISO 527 |
| Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
| Izod Impact, Notched (ISO) | 6.20 kJ/m² | 2.95 ft-lb/in² | 1A; ISO 180 |
| Charpy Impact, Notched | 0.620 J/cm² | 2.95 ft-lb/in² | 1eA; ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Heat Capacity | 1.48 J/g-°C | 0.354 BTU/lb-°F | |
| Melting Point | 167 °C | 333 °F | 10°C/min.; ISO 3146 |
| Maximum Service Temperature, Air | 100 °C | 212 °F | |
| Deflection Temperature at 1.8 MPa (264 psi) | 110 °C | 230 °F | ISO 75 |
| Vicat Softening Point | 154 °C | 309 °F | 50 N; ISO 306 |
| Flammability, UL94 | HB @Thickness 3.20 mm |
HB @Thickness 0.126 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+15 ohm | 1.00e+15 ohm | IEC 60093 |
| Dielectric Constant | 3.9 @Frequency 1e+6 Hz |
3.9 @Frequency 1e+6 Hz |
IEC 60250 |
| Dissipation Factor | 0.0085 @Frequency 1e+6 Hz |
0.0085 @Frequency 1e+6 Hz |
IEC 60250 |
| Comparative Tracking Index | 600 V | 600 V | IEC 112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 180 - 230 °C | 356 - 446 °F | Barrel temperature |
| Mold Temperature | 60.0 - 120 °C | 140 - 248 °F |