Material Notes:
Uses: Electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 75.0 MPa
10900 psi
Elongation at Break 4.0 %
4.0 %
Tensile Modulus 7.60 GPa
1100 ksi
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 20.0 °C
13.9 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
Deflection Temperature at 1.8 MPa (264 psi) 147 °C
297 °F
Vicat Softening Point 110 °C