| Category | Polymer , Thermoplastic , Elastomer, TPE , Polyester TPE , Polyester, TP |
| Manufacturer | Barlog Plastics |
| Trade Name | KEBAFLEX |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Barlog Plastics KEBAFLEX P D55.1 Polyester-Elastomer, Shore D55.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.012 cm/cm | 0.012 in/in | ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 55 | 55 | |
| Tensile Strength at Break | 35.0 MPa | 5080 psi | ISO 527-1 |
| Elongation at Break | >= 600 % | >= 600 % | ISO 527-1 |
| Charpy Impact, Notched | NB | NB | ISO 179-1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 200 °C | 392 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 70.0 °C | 158 °F | ISO 75-1/-2 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Resin Type | TPC-ET |