Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Beijing Chemical Industry KAIFA® GL1200 ABS General Purpose Grade

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Beijing Chemical Industry Research Institute (Group)
Trade Name KAIFA®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Chemical Industry KAIFA® GL1200 ABS General Purpose Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Middle impact, Good mechanical strength, High flexural strengthInformation provided by Beijing Chemical Industry Research Institute (Group)
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
24 hr; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 0.220 J/cm

@Thickness 3.20 mm
0.412 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 89.0 °C
192 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Processing Temperature 180 - 230 °C
356 - 446 °F
Resin Temp.
Rear Barrel Temperature 190 °C
374 °F
Middle Barrel Temperature 210 °C
410 °F
Front Barrel Temperature 220 °C
428 °F
Nozzle Temperature 215 °C
419 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 - 90.0 °C

@Thickness 30.0 mm
176 - 194 °F

@Thickness 1.18 in
Dry Time 4 hour

@Thickness 30.0 mm
4 hour

@Thickness 1.18 in
Injection Pressure 80.0 - 130 MPa
11600 - 18900 psi
injection speed: 80 - 120 rpm
Back Pressure 1.00 - 2.00 MPa
145 - 290 psi
Mold Pressure
Screw Speed 100 rpm
100 rpm