| Category | Polymer , Thermoplastic , Nylon |
| Manufacturer | Beijing Evergrow Resources |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Beijing Evergrow Resources Oilon.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.15 g/cc | 0.0415 lb/in³ | GB1033 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 80 - 85 | 80 - 85 | GB3398 |
| Ball Indentation Hardness | 150 MPa | 21800 psi | GB3398 |
| Tensile Strength at Break | 75.3 MPa | 10900 psi | GB/T 1040 |
| Elongation at Yield | 22.7 % | 22.7 % | GB/T 1040 |
| Modulus of Elasticity | 3.13 GPa | 454 ksi | GB/T 1040 |
| Flexural Strength | 90.7 MPa | 13200 psi | GB9341 |
| Compressive Strength | 85.0 - 100 MPa | 12300 - 14500 psi | GB/T 1040 |
| Izod Impact, Notched (ISO) | 6.40 kJ/m² | 3.05 ft-lb/in² | GBT1043 |
| Coefficient of Friction | 0.113 | 0.113 | GB3360 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 75.0 µm/m-°C | 41.7 µin/in-°F | GB1036 |
| Melting Point | 223 °C | 433 °F | HG/T2235 |
| Heat Distortion Temperature | 125 °C | 257 °F | GB1634 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | Volume; GB1410 |
| Arc Resistance | 600 sec | 600 sec | ASTM D112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Moisture Content | 1.8 - 2.0 % | 1.8 - 2.0 % | in air |
| 6.3 - 6.5 % | 6.3 - 6.5 % | in water |