Bostik 6332 Quick Setup EVA Glue Stick

Category Polymer , Adhesive , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Bostik
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bostik 6332 Quick Setup EVA Glue Stick.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Bostik 6332 Quick Setup EVA Glue StickShort open time and quick set up. Low viscosity. Easy to gun. Withstands elevated temperatures.
Physical Properties Metric English Comments
Viscosity 2000 cP

@Temperature 177 °C
2000 cP

@Temperature 350 °F
Typical
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 77.2 °C
171 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Processing Properties Metric English Comments
Pot Life 0.15 - 0.20 min
0.15 - 0.20 min
Open Time
Descriptive Properties Value Comments
Color Straw / opaque