Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic IPS610BK Electric Conducting HIPS, Extrusion

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic IPS610BK Electric Conducting HIPS, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Index of Compound 6.0 - 8.0 g/10 min
6.0 - 8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 102
102
ASTM D785
Tensile Strength, Yield 37.4 MPa
5420 psi
ASTM D638
Flexural Yield Strength 58.8 MPa
8530 psi
ASTM D790
Izod Impact, Notched 0.883 J/cm
1.65 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C
172 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1e+05
1e+05
ASTM D257