| Category | Polymer , Thermoplastic , Nylon , Nylon 46 |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Stanyl® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DSM Stanyl® TW271B3 (PA46+PTFE)-CF15.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.32 g/cc | 0.0477 lb/in³ | dry; ISO 1183 |
| Moisture Absorption | 2.60 % | 2.60 % | Sim. To ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 120 MPa | 17400 psi | cond; ISO 527-1/-2 |
| 185 MPa | 26800 psi | dry; ISO 527-1/-2 | |
| 76.0 MPa @Temperature 200 °C |
11000 psi @Temperature 392 °F |
ISO 527-1/-2 | |
| 84.0 MPa @Temperature 180 °C |
12200 psi @Temperature 356 °F |
ISO 527-1/-2 | |
| 92.0 MPa @Temperature 160 °C |
13300 psi @Temperature 320 °F |
ISO 527-1/-2 | |
| 108 MPa @Temperature 120 °C |
15700 psi @Temperature 248 °F |
ISO 527-1/-2 | |
| Elongation at Break | 2.0 % | 2.0 % | dry; ISO 527-1/-2 |
| 5.0 % | 5.0 % | cond; ISO 527-1/-2 | |
| 5.0 % @Temperature 120 °C |
5.0 % @Temperature 248 °F |
ISO 527-1/-2 | |
| 5.0 % @Temperature 160 °C |
5.0 % @Temperature 320 °F |
ISO 527-1/-2 | |
| 5.0 % @Temperature 180 °C |
5.0 % @Temperature 356 °F |
ISO 527-1/-2 | |
| 5.0 % @Temperature 200 °C |
5.0 % @Temperature 392 °F |
ISO 527-1/-2 | |
| Tensile Modulus | 6.70 GPa | 972 ksi | cond; ISO 527-1/-2 |
| 12.5 GPa | 1810 ksi | dry; ISO 527-1/-2 | |
| 5.10 GPa @Temperature 200 °C |
740 ksi @Temperature 392 °F |
ISO 527-1/-2 | |
| 5.40 GPa @Temperature 180 °C |
783 ksi @Temperature 356 °F |
ISO 527-1/-2 | |
| 5.70 GPa @Temperature 160 °C |
827 ksi @Temperature 320 °F |
ISO 527-1/-2 | |
| 6.30 GPa @Temperature 120 °C |
914 ksi @Temperature 248 °F |
ISO 527-1/-2 | |
| Flexural Modulus | 5.80 GPa | 841 ksi | cond; ISO 178 |
| 11.0 GPa | 1600 ksi | dry; ISO 178 | |
| Izod Impact Resistance | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 180/1A |
| 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 180/1A | |
| Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
| Charpy Impact, Notched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | dry; ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | dry; ISO 11359-1/-2 |
| Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 1.8 MPa (264 psi) | 290 °C | 554 °F | dry; ISO 75-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1000 ohm-cm | 1000 ohm-cm | dry; IEC 60093 |