Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Linear Mold Shrinkage 0.012 cm/cm

@Thickness 3.17 mm
0.012 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Modulus 1.795 GPa
260.3 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
3.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 252 °C
486 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648