Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&

Category Polymer , Thermoplastic , Polyester, TP , Polytrimethylene Terephthalate (PTT)
Manufacturer DuPont Performance Polymers
Trade Name Sorona®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good strength stiffness and low warpage and superior surfacInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 142 MPa
20600 psi
ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
ISO 527-1/-2
Tensile Modulus 10.6 GPa
1540 ksi
ISO 527-1/-2
Flexural Strength 215 MPa
31200 psi
ISO 178
Flexural Modulus 9.40 GPa
1360 ksi
ISO 178
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 227 °C
441 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 226 °C
439 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
IEC 60695-11-10
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
IEC 60695-11-10
Oxygen Index 21 %
21 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Surface Resistance 3.00e+14 ohm
3.00e+14 ohm
IEC 60093
Dielectric Constant 4.1

@Frequency 1.00e+6 Hz
4.1

@Frequency 1.00e+6 Hz
IEC 60250
4.3

@Frequency 100 Hz
4.3

@Frequency 100 Hz
IEC 60250
Dielectric Strength 32.0 kV/mm
813 kV/in
IEC 60243-1
Dissipation Factor 0.0015

@Frequency 100 Hz
0.0015

@Frequency 100 Hz
IEC 60250
0.0155

@Frequency 1.00e+6 Hz
0.0155

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 350 V
350 V
IEC 60112
Descriptive Properties Value Comments
Part Marking Code >PTT-GF30<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PTT-GF30
Users viewing this material also viewed the following: