| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.58 g/cc | 0.0571 lb/in³ | DAM; ISO 1183 |
| Filler Content | 50 % | 50 % | DAM |
| Water Absorption | 1.4 % @Temperature 23.0 °C |
1.4 % @Temperature 73.4 °F |
Equilibrium 50%RH; DAM; ASTM D570 |
| 1.4 % @Temperature 23.0 °C |
1.4 % @Temperature 73.4 °F |
Equilibrium 50%RH; DAM; ISO 62 | |
| 4.5 % @Temperature 23.0 °C |
4.5 % @Temperature 73.4 °F |
Saturation, immersed; DAM; ASTM D570 | |
| 4.5 % @Temperature 23.0 °C |
4.5 % @Temperature 73.4 °F |
Saturation, immersed; DAM; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.0033 cm/cm @Thickness 2.00 mm |
0.0033 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.0058 cm/cm @Thickness 2.00 mm |
0.0058 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 170 MPa @Temperature 23.0 °C |
24700 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 233 MPa @Temperature 23.0 °C |
33800 psi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Elongation at Break | 2.2 % @Temperature 23.0 °C |
2.2 % @Temperature 73.4 °F |
DAM; ISO 527 |
| 3.3 % @Temperature 23.0 °C |
3.3 % @Temperature 73.4 °F |
50%RH; ISO 527 | |
| Tensile Modulus | 12.0 GPa @Temperature 23.0 °C |
1740 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 15.5 GPa @Temperature 23.0 °C |
2250 ksi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Flexural Modulus | 11.1 GPa @Temperature 23.0 °C |
1610 ksi @Temperature 73.4 °F |
50%RH; ISO 178 |
| 14.3 GPa @Temperature 23.0 °C |
2070 ksi @Temperature 73.4 °F |
DAM; ISO 178 | |
| Charpy Impact Unnotched | 9.00 J/cm² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
| 9.80 J/cm² @Temperature 23.0 °C |
46.6 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eU | |
| 10.0 J/cm² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU | |
| 11.0 J/cm² @Temperature -30.0 °C |
52.3 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU | |
| Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
| 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA | |
| 2.10 J/cm² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA | |
| 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA | |
| Tensile Creep Modulus, 1 hour | 9400 MPa @Temperature 23.0 °C |
1.36e+6 psi @Temperature 73.4 °F |
50%RH; ISO 899 |
| Tensile Creep Modulus, 1000 hours | 7300 MPa @Temperature 23.0 °C |
1.06e+6 psi @Temperature 73.4 °F |
50%RH; ISO 899 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 23.0 - 55.0 °C |
278 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 23.0 - 55.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
| Melting Point | 219 °C | 426 °F | 10°C/min; DAM; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 219 °C | 426 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 212 °C | 414 °F | DAM; ISO 75-1/-2 |
| Flammability, UL94 | HB @Thickness 3.00 mm |
HB @Thickness 0.118 in |
DAM; IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 5.00e+12 ohm @Temperature 23.0 °C |
5.00e+12 ohm @Temperature 73.4 °F |
50%RH; IEC 60093 |
| Comparative Tracking Index | 380 V @Temperature 23.0 °C |
380 V @Temperature 73.4 °F |
DAM; IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 270 °C | 518 °F | DAM; Optimum |
| 260 - 280 °C | 500 - 536 °F | DAM | |
| Mold Temperature | 70.0 - 120 °C | 158 - 248 °F | DAM |
| 100 °C | 212 °F | DAM; optimum | |
| Drying Temperature | 80.0 °C | 176 °F | DAM |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
| Moisture Content | <= 0.20 % | <= 0.20 % | DAM |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Black Color | DAM |
| Features | Heat Stabilized | DAM |
| Lubricated | DAM | |
| Filler | Glass fiber | DAM |
| Forms | Pellets | DAM |
| Generic | Nylon 6 | DAM |
| Material Status | Preliminary Data | DAM |
| Part Marking Code | >PA6-GF50< | ISO 11469; DAM |
| Processing Method | Injection Molding | DAM |
| Product Category | Glass Reinforced Resins | DAM |
| Region Available - Global | Yes | DAM |
| Resin Identification | PA6-GF50 | ISO 1043; DAM |
| RoHS Compliance | Contact Manufacturer | DAM |