Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Unreinforced Polyamide 612 Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
DAM; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.0 MPa
7830 psi
50%RH; ISO 527-1/-2
62.0 MPa
8990 psi
DAM; ISO 527-1/-2
Elongation at Yield 4.5 %
4.5 %
DAM; ISO 527-1/-2
18 %
18 %
50%RH; ISO 527-1/-2
Tensile Modulus 1.70 GPa
247 ksi
50%RH; ISO 527-1/-2
2.40 GPa
348 ksi
DAM; ISO 527-1/-2
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
DAM; ISO 179/1eA
0.400 J/cm²
1.90 ft-lb/in²
50%RH; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
DAM; 10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Delivery Form Pellets
Part Marking Code >PA612<
ISO 11469
Processing Injection Moulding
Other Extrusion
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PA612
ISO 1043