Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® FG 47 NL nat 6028 PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® FG 47 NL nat 6028 PA6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product description: Grilon FG 47 NL natural 6028 is a modified, high viscosity Polyamide 6, which contains also slip and nucleating agents. Grilon FG 47 NL natural 6028 shows following improvements compared to standard Polyamide 6: Better flavor and gas barrierBetter optical propertiesReduced oxygen and moisture permeationBetter thermoforming with less corner thinning and better impact behavior after thermoformingHigher bonding to colors and tie layers Application examples: Grilon FG 47 NL natural 6028 is used in different extrusion processes for the production of films, sheets and containers. Thermoforming films for food (bags, trays and lidding films) at increased humidity.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 9.0 %
9.0 %
ISO 62
Moisture Absorption 3.00 %
3.00 %
ISO 62
Water Vapor Transmission 10.0 g/m²/day
0.644 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
Oxygen Transmission Rate 25.0 cc/m²/day
1.61 cc/100 in²/day
23°C/0%r.h.; DIS 15105-1/-2
40.0 cc/m²/day
2.58 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
Carbon Dioxide Transmission 80.0 cc-mm/m²-24hr-atm
203 cc-mil/100 in²-24hr-atm
23°C/0%r.h.; DIS 15105-1/-2
200 cc-mm/m²-24hr-atm
508 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
Melt Flow 15 g/10 min
15 g/10 min
(MVR) [cm³/10min]; ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 40.0 MPa
5800 psi
ISO 527-3
Film Tensile Strength at Yield, TD 40.0 MPa
5800 psi
ISO 527-3
Film Elongation at Break, MD 600 %
600 %
ISO 527-3
Film Elongation at Break, TD 900 %
900 %
ISO 527-3
Film Elongation at Yield, MD 10 %
10 %
ISO 527-3
Film Elongation at Yield, TD 7.0 %
7.0 %
ISO 527-3
Tensile Modulus 1.10 GPa
160 ksi
conditioned; ISO 527-1/-2
3.00 GPa
435 ksi
dry; ISO 527-1/-2
Tear Strength 50.0 kN/m
285 pli
Trouser Tear resistance MD; ISO 6383-1
50.0 kN/m
285 pli
Trouser Tear resistance TD; ISO 6383-1
Elmendorf Tear Strength MD 1530 g
1530 g
ISO 6383-2
Elmendorf Tear Strength TD 1530 g
1530 g
ISO 6383-2
Film Tensile Strength at Break, MD 100 MPa
14500 psi
ISO 527-3
Film Tensile Strength at Break, TD 90.0 MPa
13100 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Optical Properties Metric English Comments
Gloss 100 %
100 %
60°; ISO 2813
Descriptive Properties Value Comments
Food contact EU Requirements
FDA
Form Granules
Packaging Medical packaging
Non oriented film
Oriented film
Tubes
Processing Blown Film Extrusion
Extrusion - blow molding
Film Extrusion
Other Extrusion
Product Attributes Barrier Properties
High viscosity
Nucleated