Fainplast Compounds FK 90 Flexible PVC, Insulation Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds FK 90 Flexible PVC, Insulation Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General purposes
Physical Properties Metric English Comments
Density 1.46 - 1.50 g/cc
0.0527 - 0.0542 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 92
88 - 92
ISO R 868
Tensile Strength at Break >= 15.0 MPa
>= 2180 psi
ISO R 527
Elongation at Break >= 240 %
>= 240 %
ISO R 527
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm

@Temperature 23.0 °C
1.00e+14 ohm-cm

@Temperature 73.4 °F
ASTM D257
Descriptive Properties Value Comments
Thermal Stability (minutes) 50
CEI 20-34/3-2