Fainplast Compounds HGA 40 Flexible PVC, Sheathing for High Temperatures

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds HGA 40 Flexible PVC, Sheathing for High Temperatures.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Sheath high L.O.I.
Physical Properties Metric English Comments
Density 1.51 - 1.55 g/cc
0.0546 - 0.0560 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Hardness, Shore A 89 - 93
89 - 93
ISO R 868
Tensile Strength at Break >= 13.0 MPa
>= 1890 psi
ISO R 527
Elongation at Break >= 200 %
>= 200 %
ISO R 527
Thermal Properties Metric English Comments
Oxygen Index 40 %
40 %
ISO 4589
Descriptive Properties Value Comments
Thermal Stability (minutes) 120
CEI 20-34/3-2