Global TPO-28T Talc Filled TPO Grade

Category Polymer , Thermoplastic , TPO
Manufacturer Global Polymers Corporation
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Global TPO-28T Talc Filled TPO Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Melt Flow 12 g/10 min
12 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256