| Category | Polymer , Adhesive , Thermoset , Epoxy |
| Manufacturer | ITW Devcon |
| Trade Name | 10 minute™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | ITW Devcon 10 minuteâ„¢ Epoxy, Black.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 90000 cP | 90000 cP | Mixed Viscosity |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Elongation at Break | 5.0 % | 5.0 % | |
| Adhesive Bond Strength | 16.5 MPa | 2400 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
| Tensile Impact Strength | 21.0 kJ/m² | 10.0 ft-lb/in² | |
| Peel Strength | 3.51 - 4.38 kN/m | 20.0 - 25.0 pli |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 93.3 °C | 200 °F | dry |
| Minimum Service Temperature, Air | -55.0 °C | -67.0 °F | dry |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 10.0 min | 0.167 hour | Working time |
| 20.0 min | 0.333 hour | Fixture time | |
| 90.0 min | 1.50 hour | Functional cure |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Mix ratio (Resin:Hardener) | 1:1 |