| Category | Polymer , Adhesive , Thermoset , Epoxy |
| Manufacturer | ITW Devcon |
| Trade Name | Safety Clear Coat™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | ITW Devcon Safety Clear Coatâ„¢ Epoxy, Water Clear.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 3500 cP | 3500 cP | Mixed Viscosity |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Elongation at Break | 150 % | 150 % | |
| Adhesive Bond Strength | 8.27 MPa | 1200 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
| Tensile Impact Strength | 31.5 kJ/m² | 15.0 ft-lb/in² | |
| Peel Strength | 8.77 kN/m | 50.0 pli |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 79.4 °C | 175 °F | dry |
| Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | dry |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 90 % | 90 % | clear; thickness not quantified |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 30.0 - 40.0 min | 0.500 - 0.667 hour | Working time |
| 240 min | 4.00 hour | Fixture time | |
| 480 - 600 min | 8.00 - 10.0 hour | Functional cure |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Mix ratio (Resin:Hardener) | 1:1 |