Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kraton® D1112P (SIS) Linear Block Copolymer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Kraton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D1112P (SIS) Linear Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
(SIS) styrene-isoprene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact qualities of the material, both at room and low temperature. This KRATON polymer meets FDA regulations as articles or as ingredients in articles intended for food contact. FDA clearances vary from one grade to another. For specific clearances, letters of certification will be provided on request.Applications: modified asphalts, thermoplastic and thermoset polymer modification, adhesives, sealants, coatings, sporting goods, film, and general elastomer compounding.Information provided by the manufacturer, Kraton® Polymers.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
Brookfield Viscosity 900 cP

@Temperature 25.0 °C
900 cP

@Temperature 77.0 °F
Toluene solution. Neat polymer concentration, 25%w.
Melt Flow 23 g/10 min
23 g/10 min
Mechanical Properties Metric English Comments
Hardness, Shore A 25
25
10 seconds. Typical values on polymer compression molded at 150°C (300°F).
Tensile Strength, Ultimate 10.34 MPa
1500 psi
Tensile tester jaw separation 10 in/min (25.4 cm/min). Typical properties based on film cast from toluene solution.; ASTM D412
Elongation at Break 1400 %
1400 %
Tensile tester jaw separation 10 in/min (25.4 cm/min); ASTM D412
300% Modulus 0.000483 GPa
0.0701 ksi
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 - 1.00e+16 ohm-cm
1.00e+14 - 1.00e+16 ohm-cm
Dielectric Strength 11.81 - 39.37 kV/mm
300.0 - 1000 kV/in
Processing Properties Metric English Comments
Processing Temperature 150 - 200 °C
302 - 392 °F