Material Notes:
Lucite® XL continuous-cast cross-linked acrylic sheet is specially formulated for deep-draw thermoforming. It is used primarily for production of spas.Benefits: Smooth surface; Infinite colors and effects; Hardwearing; Exceptional quality; 100% recyclable; Enhanced functionalityInformation provided by Lucite International
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Water Absorption 0.25 %
0.25 %
ASTM D570
Linear Mold Shrinkage <= 0.025 cm/cm
<= 0.025 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
ASTM D785 Procedure A
Tensile Strength 62.0 - 69.0 MPa
8990 - 10000 psi
specimen type 1, 5 mm/mn; ASTM D638
Elongation at Break 4.0 - 5.0 %
4.0 - 5.0 %
Modulus of Elasticity 3.172 GPa
460.1 ksi
Flexural Strength 110.3 MPa
16000 psi
ASTM D790 (Method 1, Procedure A)
Compressive Yield Strength 111 MPa
16100 psi
ASTM D695
Shear Strength 59.6 MPa
8640 psi
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256 method C
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C
38.9 µin/in-°F
ASTM D696
Specific Heat Capacity 1.47 J/g-°C
0.351 BTU/lb-°F
ASTM C351
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
ASTM C177-76
Maximum Service Temperature, Air 80.0 °C
176 °F
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C
187 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistance <= 1.00e+14 ohm

@Temperature 28.0 °C
<= 1.00e+14 ohm

@Temperature 82.4 °F
75% RH; ASTM D257
Dielectric Constant 3.0

@# of Cycles 1000
3.0

@# of Cycles 1000
ASTM D150
3.0

@# of Cycles 1.00e+6
3.0

@# of Cycles 1.00e+6
ASTM D150
4.0

@# of Cycles 60.0
4.0

@# of Cycles 60.0
ASTM D150
Dielectric Strength 20.0 kV/mm
508 kV/in
short time test; ASTM D149
Processing Properties Metric English Comments
Processing Temperature 170 - 190 °C
338 - 374 °F
thermoforming temperature