Momentive Performance Materials RTV5229 Neutral Cure, One Component RTV Adhesive Sealant

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials RTV5229 Neutral Cure, One Component RTV Adhesive Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
RTV5220 series sealants are alkoxy neutral cure, one-component, ready to use silicone adhesive sealants exhibiting low modulus/high elongation that will maintain a strong bond even when exposed to extreme movement. RTV5220 series3 sealants are true neutral curing silicone sealants that release methyl alcohol during cure while exposed to atmospheric moisture at room temperature. Key Performance Properties: A non-corrosive curing process that does not produce exothermic heat or corrosive by-products. Can be used on most corrosion-sensitive electrical and electronic equipment with no adverse effectLow modulus/high elongation sealant with primerless adhesion to most metals, painted surfaces and plastics, including polycarbonate and acrylicCompatible with most sensitive metals and plasticsWithstands exposure to harsh environments such as chemical, ozone, moisture and weatheringGood tear resistanceEasy handling with no mixing, heating or solvent hazardsLow odor cure by-productUL recognized component - file number E-36952 Retain elastomeric properties at temperatures of -75° to 1400°FApplications: The RTV5220 series are low modulus/high elongation, alkoxy neutral one-part silicone sealants designed for use with glass, ceramic, metals, and plastics. RTV5220 sealants are well suited when bonding materials with large thermal coefficient of expansion properties, and dissimilar materials.Because they are one-part products, there is no mixing required. The sealant can be easily dispensed from simple bulk dispensing pumps or cartridges. Base/catalyst ratio control, static mixer maintenance, butterfly testing for mix uniformity, yield loss from base purging, and other activities/costs associated with two-part sealants are eliminated.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 26
26
Tensile Strength, Ultimate 2.600 MPa
377.1 psi
Elongation at Break 750 %
750 %
Electrical Properties Metric English Comments
Volume Resistivity 5.40e+15 ohm-cm
5.40e+15 ohm-cm
Dielectric Constant 3.9

@Frequency 60 Hz
3.9

@Frequency 60 Hz
Dielectric Strength 16.5 kV/mm
419 kV/in
Dissipation Factor 0.0010

@Frequency 60 Hz
0.0010

@Frequency 60 Hz
Processing Properties Metric English Comments
Cure Time 200 min
3 hour
Tack-free
1440 min
24.0 hour
To depth of 3.2 mm
Descriptive Properties Value Comments
Application rate 185 g/min
Color Gray
Sag/Slump 2.5 mm
Tooling time 30 min