Material Notes:
Molded Plaque Properties. Features: High molecular weight, excellent ESCR, impact strength, high rigidity.Applications: large-part blow-molding, trash cans, drums, jerry cans, fuel tanks.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
F50, Condition B, ASTM D1693, 100% Igepal AND Condition A, 20% Igepal
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Elongation at Break 820 %
820 %
ASTM D638
Flexural Modulus 1.28 GPa
186 ksi
ASTM D790
Izod Impact, Notched 3.90 J/cm
7.31 ft-lb/in
Notched/Unnotched not specified; ASTM D256
Tensile Impact Strength 320 kJ/m²
152 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D696
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
Users viewing this material also viewed the following: