Material Notes:
FDA approved extrusion grade for film.Information provided by NYCOA, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 2.0 %
2.0 %
ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 72.0 MPa
10400 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Yield Strength 89.0 MPa
12900 psi
ASTM D790
Flexural Modulus 2.372 GPa
344.0 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 199 °C
390 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F
Rear Barrel Temperature 200 °C
392 °F
Middle Barrel Temperature 230 °C
446 °F
Front Barrel Temperature 250 °C
482 °F
Nozzle Temperature 250 °C
482 °F
Mold Temperature 80.0 °C
176 °F
Drying Temperature 76.0 °C
169 °F