Overview of materials for Acrylic, Optical Sheet

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Optical Sheet
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Acrylic, Optical Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.15 - 1.19 g/cc
0.0415 - 0.0430 lb/in³
Average value: 1.18 g/cc Grade Count:14
Water Absorption 0.200 - 0.400 %
0.200 - 0.400 %
Average value: 0.317 % Grade Count:6
Linear Mold Shrinkage 0.00200 - 0.00600 cm/cm
0.00200 - 0.00600 in/in
Average value: 0.00425 cm/cm Grade Count:4
Mechanical Properties Metric English Comments
Hardness, Rockwell M 46.0 - 96.0
46.0 - 96.0
Average value: 81.6 Grade Count:7
Hardness, Rockwell R 106 - 110
106 - 110
Average value: 108 Grade Count:5
Tensile Strength, Yield 37.9 - 72.0 MPa
5500 - 10400 psi
Average value: 55.2 MPa Grade Count:11
Elongation at Break 4.50 - 5.80 %
4.50 - 5.80 %
Average value: 4.87 % Grade Count:6
Modulus of Elasticity 1.52 - 3.38 GPa
220 - 490 ksi
Average value: 2.46 GPa Grade Count:14
Flexural Yield Strength 57.0 - 117 MPa
8270 - 17000 psi
Average value: 97.6 MPa Grade Count:13
Flexural Modulus 1.86 - 3.38 GPa
270 - 490 ksi
Average value: 2.76 GPa Grade Count:10
Compressive Yield Strength 117 - 124 MPa
17000 - 18000 psi
Average value: 119 MPa Grade Count:3
Izod Impact, Notched 0.149 - 1.10 J/cm
0.280 - 2.06 ft-lb/in
Average value: 0.425 J/cm Grade Count:7
0.200 - 0.500 J/cm

@Temperature -18.0 - -18.0 °C
0.375 - 0.937 ft-lb/in

@Temperature -0.400 - -0.400 °F
Average value: 0.275 J/cm Grade Count:4
Izod Impact, Unnotched 0.320 - 0.587 J/cm
0.600 - 1.10 ft-lb/in
Average value: 0.427 J/cm Grade Count:5
Gardner Impact 0.450 - 5.30 J
0.332 - 3.91 ft-lb
Average value: 2.49 J Grade Count:4
Falling Dart Impact 8.13 - 13.6 J
6.00 - 10.0 ft-lb
Average value: 10.3 J Grade Count:5
Thermal Properties Metric English Comments
CTE, linear 52.2 - 101 µm/m-°C
29.0 - 56.0 µin/in-°F
Average value: 75.7 µm/m-°C Grade Count:14
Thermal Conductivity 0.130 - 0.190 W/m-K
0.900 - 1.32 BTU-in/hr-ft²-°F
Average value: 0.160 W/m-K Grade Count:4
Maximum Service Temperature, Air 60.0 - 88.0 °C
140 - 190 °F
Average value: 74.2 °C Grade Count:8
Deflection Temperature at 1.8 MPa (264 psi) 76.7 - 98.9 °C
170 - 210 °F
Average value: 87.7 °C Grade Count:14
Vicat Softening Point 105 - 115 °C
221 - 239 °F
Average value: 110 °C Grade Count:4
Minimum Service Temperature, Air -55.0 - -34.0 °C
-67.0 - -29.2 °F
Average value: -51.5 °C Grade Count:4
Flammability, UL94 HB
HB
Grade Count:5
Flame Spread 15.2 - 25.9 mm/min
0.600 - 1.02 in/min
Average value: 20.5 mm/min Grade Count:3
Optical Properties Metric English Comments
Refractive Index 1.46 - 1.49
1.46 - 1.49
Average value: 1.48 Grade Count:5
Haze 1.00 - 3.00 %
1.00 - 3.00 %
Average value: 1.78 % Grade Count:7
Gloss 90.0 %
90.0 %
Average value: 90.0 % Grade Count:4
Transmission, Visible 63.0 - 92.0 %
63.0 - 92.0 %
Average value: 90.3 % Grade Count:10
Electrical Properties Metric English Comments
Shielding Effectiveness 40.0 - 120 dB
40.0 - 120 dB
Average value: 73.8 dB Grade Count:3
Processing Properties Metric English Comments
Processing Temperature 143 - 160 °C
289 - 320 °F
Average value: 156 °C Grade Count:4