Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Masterbatch Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.913 - 1.19 g/cc
0.0330 - 0.0430 lb/in³
Average value: 0.940 g/cc Grade Count:29
Particle Size 150 - 1200 µm
150 - 1200 µm
Average value: 404 µm Grade Count:26
Melt Flow 0.200 - 155 g/10 min
0.200 - 155 g/10 min
Average value: 48.3 g/10 min Grade Count:27
Mechanical Properties Metric English Comments
Hardness, Shore D 40.0 - 50.0
40.0 - 50.0
Average value: 44.0 Grade Count:16
Tensile Strength, Ultimate 8.00 - 9.00 MPa
1160 - 1310 psi
Average value: 8.50 MPa Grade Count:4
Tensile Strength, Yield 8.00 - 9.00 MPa
1160 - 1310 psi
Average value: 8.50 MPa Grade Count:4
Elongation at Break 90.0 - 100 %
90.0 - 100 %
Average value: 97.1 % Grade Count:21
Modulus of Elasticity 0.0900 - 0.200 GPa
13.1 - 29.0 ksi
Average value: 0.127 GPa Grade Count:12
Thermal Properties Metric English Comments
Melting Point 100 - 140 °C
212 - 284 °F
Average value: 107 °C Grade Count:26
Vicat Softening Point 68.0 - 86.0 °C
154 - 187 °F
Average value: 77.5 °C Grade Count:26
Brittleness Temperature -45.0 - -25.0 °C
-49.0 - -13.0 °F
Average value: -35.0 °C Grade Count:4
Processing Properties Metric English Comments
Processing Temperature 200 °C
392 °F
Average value: 200 °C Grade Count:8