| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.992 - 1.44 g/cc | 0.0358 - 0.0520 lb/in³ | Average value: 1.21 g/cc Grade Count:211 |
| Viscosity | 30.0 - 5500 cP | 30.0 - 5500 cP | Average value: 915 cP Grade Count:21 |
| 28000 - 130000 cP @Temperature 204 - 204 °C |
28000 - 130000 cP @Temperature 399 - 399 °F |
Average value: 83800 cP Grade Count:4 | |
| Maximum Moisture Content | 0.0200 - 0.0500 | 0.0200 - 0.0500 | Average value: 0.0329 Grade Count:35 |
| Linear Mold Shrinkage | 0.00200 - 0.0250 cm/cm | 0.00200 - 0.0250 in/in | Average value: 0.00748 cm/cm Grade Count:72 |
| Linear Mold Shrinkage, Transverse | -0.00200 - 0.00900 cm/cm | -0.00200 - 0.00900 in/in | Average value: 0.00513 cm/cm Grade Count:12 |
| Melt Flow | 4.00 - 90.0 g/10 min | 4.00 - 90.0 g/10 min | Average value: 31.9 g/10 min Grade Count:51 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 40.0 - 98.0 | 40.0 - 98.0 | Average value: 85.3 Grade Count:159 |
| Hardness, Shore D | 12.0 - 79.0 | 12.0 - 79.0 | Average value: 49.5 Grade Count:122 |
| Tensile Strength, Ultimate | 1.35 - 72.1 MPa | 196 - 10400 psi | Average value: 38.8 MPa Grade Count:205 |
| 28.91 - 49.0 MPa @Temperature 70.0 - 100 °C |
4193 - 7110 psi @Temperature 158 - 212 °F |
Average value: 43.3 MPa Grade Count:1 | |
| 28.91 - 49.0 MPa @Time 0.000 - 3.63e+6 sec |
4193 - 7110 psi @Time 0.000 - 1010 hour |
Average value: 43.3 MPa Grade Count:1 | |
| Tensile Strength, Yield | 1.10 - 66.4 MPa | 160 - 9630 psi | Average value: 14.1 MPa Grade Count:181 |
| Elongation at Break | 10.0 - 1580 % | 10.0 - 1580 % | Average value: 550 % Grade Count:211 |
| Modulus of Elasticity | 0.00300 - 0.870 GPa | 0.435 - 126 ksi | Average value: 0.136 GPa Grade Count:32 |
| Flexural Yield Strength | 2.61 - 62.7 MPa | 379 - 9100 psi | Average value: 24.2 MPa Grade Count:6 |
| Flexural Modulus | 0.0276 - 1.21 GPa | 4.00 - 175 ksi | Average value: 0.223 GPa Grade Count:28 |
| Resilience | 30.0 - 60.0 | 30.0 - 60.0 | Average value: 42.3 Grade Count:22 |
| Rebound | 25.0 - 57.0 % | 25.0 - 57.0 % | Average value: 38.1 % Grade Count:45 |
| Shear Modulus | 0.0120 - 0.250 GPa | 1.74 - 36.3 ksi | Average value: 0.102 GPa Grade Count:3 |
| Izod Impact, Notched | 0.849 - 5340 J/cm | 1.59 - 10000 ft-lb/in | Average value: 3.88 J/cm Grade Count:6 |
| 0.26695 - 2.93645 J/cm @Temperature -40.0 - -40.0 °C |
0.50011 - 5.50117 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.60 J/cm Grade Count:2 | |
| Izod Impact, Unnotched | 0.961 - 5340 J/cm | 1.80 - 10000 ft-lb/in | Average value: 0.969 J/cm Grade Count:3 |
| Tear Strength | 17.5 - 285 kN/m | 100 - 1630 pli | Average value: 113 kN/m Grade Count:187 |
| Peel Strength | 0.0400 - 7.20 kN/m | 0.228 - 41.1 pli | Average value: 1.93 kN/m Grade Count:6 |
| Graves Tear Strength | 52.6 - 210 kN/m | 300 - 1200 pli | Average value: 124 kN/m Grade Count:18 |
| Taber Abrasion, mg/1000 Cycles | 0.700 - 127 | 0.700 - 127 | Average value: 34.3 Grade Count:85 |
| Compression Set | 12.0 - 90.0 % | 12.0 - 90.0 % | Average value: 33.0 % Grade Count:92 |
| 25.0 - 40.0 % @Temperature 70.0 - 70.0 °C |
25.0 - 40.0 % @Temperature 158 - 158 °F |
Average value: 42.7 % Grade Count:8 | |
| 23.0 - 80.0 % @Temperature 70.0 - 100 °C |
23.0 - 80.0 % @Temperature 158 - 212 °F |
Average value: 42.7 % Grade Count:39 | |
| 23.0 - 80.0 % @Time 79200 - 252000 sec |
23.0 - 80.0 % @Time 22.0 - 70.0 hour |
Average value: 42.7 % Grade Count:39 | |
| Tensile Set | 4.00 - 155 % | 4.00 - 155 % | Average value: 52.7 % Grade Count:46 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 117 - 171 µm/m-°C | 65.0 - 95.0 µin/in-°F | Average value: 150 µm/m-°C Grade Count:15 |
| Melting Point | 100 - 230 °C | 212 - 446 °F | Average value: 170 °C Grade Count:43 |
| Vicat Softening Point | 35.0 - 165 °C | 95.0 - 329 °F | Average value: 103 °C Grade Count:94 |
| Brittleness Temperature | -70.0 - -50.0 °C | -94.0 - -58.0 °F | Average value: -68.4 °C Grade Count:16 |
| Glass Transition Temp, Tg | -47.0 - 120 °C | -52.6 - 248 °F | Average value: -22.9 °C Grade Count:39 |
| Transformation Temperature | -27.8 - -17.2 °C | -18.0 - 1.00 °F | Average value: -22.0 °C Grade Count:3 |
| Clash Berg Stiffness Temperature | -40.0 - -5.00 °C | -40.0 - 23.0 °F | Average value: -26.4 °C Grade Count:6 |
| Flammability, UL94 | HB | HB | Grade Count:3 |
| Ring & Ball Softening Point | 161 - 179 °C | 322 - 354 °F | Average value: 170 °C Grade Count:3 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 90.0 % | 90.0 % | Average value: 90.0 % Grade Count:12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.00e+10 - 1.00e+13 ohm-cm | 1.00e+10 - 1.00e+13 ohm-cm | Average value: 3.37e+12 ohm-cm Grade Count:3 |
| Surface Resistance | 5.00e+8 - 1.00e+12 ohm | 5.00e+8 - 1.00e+12 ohm | Average value: 2.78e+11 ohm Grade Count:4 |
| Dielectric Constant | 4.10 - 7.10 | 4.10 - 7.10 | Average value: 5.73 Grade Count:3 |
| Dielectric Strength | 31.0 - 49.0 kV/mm | 787 - 1240 kV/in | Average value: 42.7 kV/mm Grade Count:3 |
| Dissipation Factor | 0.0240 - 0.200 | 0.0240 - 0.200 | Average value: 0.0557 Grade Count:3 |
| Comparative Tracking Index | 600 V | 600 V | Average value: 600 V Grade Count:6 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 155 - 216 °C | 311 - 421 °F | Average value: 195 °C Grade Count:24 |
| Nozzle Temperature | 160 - 299 °C | 320 - 570 °F | Average value: 199 °C Grade Count:75 |
| Adapter Temperature | 175 - 215 °C | 347 - 419 °F | Average value: 193 °C Grade Count:43 |
| Die Temperature | 145 - 215 °C | 293 - 419 °F | Average value: 194 °C Grade Count:56 |
| Melt Temperature | 120 - 238 °C | 248 - 460 °F | Average value: 192 °C Grade Count:108 |
| Head Temperature | 170 - 210 °C | 338 - 410 °F | Average value: 195 °C Grade Count:10 |
| Mold Temperature | 16.0 - 70.0 °C | 60.8 - 158 °F | Average value: 36.2 °C Grade Count:51 |
| Drying Temperature | 54.0 - 110 °C | 129 - 230 °F | Average value: 95.6 °C Grade Count:58 |
| Moisture Content | 0.0100 - 0.100 % | 0.0100 - 0.100 % | Average value: 0.0425 % Grade Count:20 |