PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer PolyOne Corporation
Trade Name Dynaflex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - Overmold Adhesion to Polypropylene - Suitable For Outdoor UseDynaflex™ G7410-1000-00 can be recycled as a filler or impact modifier for polyolefins, or can be recycled by grinding and reintroduction to the molding process. Similar to PP or PE recycling process, if separated appropriately, it can be recycled many times. Municipality waste stream recycle code is 7 which is designated for Other. Please contact GLS Thermoplastic Elastomers for a copy of our Recyclability Compliance letter.Color concentrates with polypropylene (PP), ethylene vinyl acetate (EVA), or low density polyethylene (PE) carriers are most suitable for coloring Dynaflex™ G7410-1000-00. Improved color dispersion can be achieved by using higher melt flow concentrates (with a melt flow from 25 - 40 g/10 min). Typical loadings for color concentrates are 1% to 5% by weight. Liquid color can be used, but mineral oil based carriers may have a significant effect on the final hardness value. Concentrates based on PVC should not be used. A high color match consistency can be obtained by using precolored compounds available from GLS. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). Regrind levels up to 20% can be used with Dynaflex™ G7410-1000-00 with minimal property loss, provided that the regrind is free of contamination. The final determination of regrind effectiveness should be determined by the customer. Dynaflex™ G7410-1000-00 has excellent melt stability. Empty the barrel for idle periods of thirty (30) minutes or longer. Drying is not Required Injection Speed: 1 to 5 in/sec 1st Stage - Boost Pressure: 250 to 650 psi 2nd Stage - Hold Pressure: 70% of Boost Hold Time (Thick Part): 4 to 10 sec Hold Time (Thin Part): 1 to 3 secInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.898 g/cc
0.898 g/cc
ASTM D792
Viscosity 14800 cP

@Shear Rate 11200 1/s,
Temperature 200 °C
14800 cP

@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
Linear Mold Shrinkage, Flow 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
ASTM D955
Melt Flow 2.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
10 sec; ASTM D2240
Tensile Strength at Break 5.17 MPa

@Temperature 23.0 °C
750 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress 2.69 MPa

@Strain 100 %,
Temperature 23.0 °C
390 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
3.55 MPa

@Strain 300 %,
Temperature 23.0 °C
515 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 500 %

@Temperature 23.0 °C
500 %

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tear Strength 28.0 kN/m
160 pli
ASTM D624
Compression Set 19 %

@Temperature 23.0 °C,
Time 79200 sec
19 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Rear Barrel Temperature 166 - 204 °C
331 - 399 °F
Middle Barrel Temperature 177 - 216 °C
351 - 421 °F
Front Barrel Temperature 182 - 221 °C
360 - 430 °F
Nozzle Temperature 182 - 221 °C
360 - 430 °F
Mold Temperature 15.6 - 26.7 °C
60.1 - 80.1 °F
Back Pressure 0.345 - 1.03 MPa
50.0 - 149 psi
Screw Speed 25 - 75 rpm
25 - 75 rpm
Descriptive Properties Value Comments
Appearance Natural Color
Features Good Colorability
Good Thermal Stability
Recyclable Material
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Suggested Max Regrind 20%
Uses Outdoor Applications
Overmolding