| Category | Polymer , Thermoplastic , Vinyl (PVC) , Chlorinated PVC (CPVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ CPVC MC550 Polyvinyl Chloride, Chlorinated (CPVC).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.53 g/cc | 1.53 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 111 | 111 | ASTM D785 |
| Tensile Strength, Yield | 48.7 MPa @Temperature 23.0 °C |
7060 psi @Temperature 73.4 °F |
ASTM D638 |
| Tensile Modulus | 2.52 GPa @Temperature 23.0 °C |
365 ksi @Temperature 73.4 °F |
Yield; ASTM D638 |
| Flexural Yield Strength | 84.8 MPa | 12300 psi | ASTM D790 |
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
| Izod Impact, Notched | 1.30 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.44 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
| Izod Impact, Notched (ISO) | 2.31 kJ/m² @Thickness 3.18 mm, Temperature 0.000 °C |
1.10 ft-lb/in² @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 97.0 °C | 207 °F | Annealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | Annealed; ASTM D648 |
| Vicat Softening Point | 98.0 °C | 208 °F | Method A 98°C.; ASTM D1525 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 200 - 207 °C | 392 - 405 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Agency Ratings | UL 94 | Pass V-0 - Not Listed |
| Forms | Pellets | |
| Generic Material | CPVC | |
| Generic Name | Polyvinyl Chloride, Chlorinated (CPVC) | |
| Processing Method | Injection Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Outdoor Applications |