Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Wire & Cable Y66A Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable Y66A Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
15 sec; ASTM D2240
Tensile Strength, Yield 15.2 MPa
2200 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 370 %
370 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
UL Temperature Rating
Brittleness Temperature -30.0 °C
-22.0 °F
ASTM D746
Oxygen Index 26 %

@Thickness 1.91 mm
26 %

@Thickness 0.0752 in
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 5.90e+14 ohm-cm
5.90e+14 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 160 - 170 °C
320 - 338 °F
Descriptive Properties Value Comments
Additive Lead Stabilizer
Agency Ratings UL QMTT2
Features Flame Retardant
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Retention of Tensile Elongation 80%
136°C, 1.91 mm; 168 hr, UL Standard
Retention of Tensile Strength 130%
136°C, 1.91 mm; 168 hr, UL Standard
Uses Flexible Cord Insulation
Wire & Cable Applications
Wire Types SJTW
STW
Users viewing this material also viewed the following: