| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 11.0 g/cc | 11.0 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | Type I, 5.1 mm/min; ASTM D638 |
| Elongation at Break | 1.0 % | 1.0 % | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 8.96 GPa | 1300 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 68.9 MPa | 9990 psi | ASTM D790 |
| Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
| Izod Impact, Notched | 0.800 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 155 °C @Thickness 6.35 mm |
311 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 260 - 288 °C | 500 - 550 °F | |
| Mold Temperature | 82.2 - 149 °C | 180 - 300 °F | |
| Drying Temperature | 79.4 °C | 175 °F | |
| Dry Time | 4.00 hour | 4.00 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | High Density | |
| Non-Toxic | ||
| Forms | Pellets | |
| Generic Material | Nylon 12 | |
| Generic Name | Polyamide 12 (Nylon 12) | |
| Processing Method | Injection Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Industrial Applications | |
| Medical/Healthcare Applications | ||
| Projectiles | ||
| Radiation Shielding | ||
| Sporting Goods | ||
| Weighting & Balancing |