Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Nymax™ GF 1200 A 43 Natural Polyamide 66 (Nylon 66)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer PolyOne Corporation
Trade Name Nymax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Nymax™ GF 1200 A 43 Natural Polyamide 66 (Nylon 66).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durability in harsh environments. These materials are available in a broad range of reinforcement levels depending upon stiffness characteristics desired and have been formulated to offer ease of processing in most standard thermoplastic processing equipmentMolded Test Bars: Dry as MoldedInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Water Absorption 0.60 %

@Thickness 3.18 mm
0.60 %

@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 221 MPa
32100 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 2.5 %
2.5 %
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 290 MPa
42100 psi
ASTM D790
Flexural Modulus 12.1 GPa
1750 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
3.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 257 °C

@Thickness 3.18 mm
495 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 252 °C

@Thickness 3.18 mm
486 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Mold Temperature 60.0 - 107 °C
140 - 225 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Appearance Natural Color
Features General Purpose
Filler / Reinforcement Glass Fiber Reinforcement
Unspecified FillerReinfor., 43% Filler by Weight
Forms Pellets
Generic Material Nylon 66
Generic Name Polyamide 66 (Nylon 66)
Processing Method Injection Molding
Regional Availability North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications
Users viewing this material also viewed the following: