Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Stat-Tech™ AS-10CP/000 Acrylonitrile Butadiene Styrene (ABS)  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Stat-Tech™ AS-10CP/000 Acrylonitrile Butadiene Styrene (ABS)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description/Features:AntistaticConductive Carbon Powder FilledInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.095 g/cc
1.095 g/cc
Calculated
Water Absorption 0.15 %

@Thickness 3.17 mm
0.15 %

@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 2.76 GPa
400 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 44.8 MPa
6500 psi
ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.800 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C
200 °F
Annealed, 0.125 in bars; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Surface Resistivity per Square 1.00e+12 ohm
1.00e+12 ohm
ASTM D257