| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.02 g/cc | 0.0368 lb/in³ | ISO 1183 |
| Water Absorption | 0.010 % | 0.010 % | immersion @23°C; ISO 62 |
| Water Absorption at Saturation | 0.010 % | 0.010 % | |
| Water Vapor Transmission | 0.0300 g/m²/day | 0.00193 g/100 in²/day | [g·mm/m<sup>2</sup>·d] @ 23°C and 85% RH; DIN 53122 |
| 0.250 g/m²/day | 0.0161 g/100 in²/day | Good barrier properties | |
| Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 245 °C |
26 g/10 min @Load 4.76 lb, Temperature 473 °F |
ISO 1133 |
| 49 g/10 min @Load 2.16 kg, Temperature 260 °C |
49 g/10 min @Load 4.76 lb, Temperature 500 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | 5mm/min; ISO 527-1, 2 |
| Elongation at Break | 1.7 % | 1.7 % | 5mm/min; ISO 527-1, 2 |
| Tensile Modulus | 3.20 GPa | 464 ksi | 1mm/min; ISO 527-1, 2 |
| Charpy Impact Unnotched | 1.30 J/cm² | 6.19 ft-lb/in² | ISO 179/1eU |
| Charpy Impact, Notched | 0.160 J/cm² | 0.761 ft-lb/in² | ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | |
| Deflection Temperature at 1.8 MPa (264 psi) | 116 °C | 241 °F | ISO 75-1, 2 |
| Glass Transition Temp, Tg | 140 °C | 284 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.53 | 1.53 | |
| Transmission, Visible | 91 % | 91 % | ISO 13468-1 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 2.2 @Frequency 1.00e+10 Hz |
2.2 @Frequency 1.00e+10 Hz |
|
| Dissipation Factor | 0.00010 @Frequency 1.00e+10 Hz |
0.00010 @Frequency 1.00e+10 Hz |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Abbe number | 58 | |
| Birefringence, nm | max 20 | |
| Optical Stress Constant, Pa-1 | from -7E-12 to -2E-12 | |
| Pencil Hardness | F | JIS K5401 |
| Resistance to Acids | Usable | |
| Resistance to Alcohols | Usable | |
| Resistance to Alkalis | Usable | |
| Resistance to Aromatic Solvents | Not Usable | |
| Resistance to Chlorinated Solvents | Not Usable | |
| Resistance to Esters | Usable | |
| Resistance to Gasoline | Not Usable | |
| Resistance to Ketones | Usable | |
| Resistance to Oils | Not Usable |